PerformanceParameter
enumerationNo description available.
Values (12)
| Value | Description |
|---|---|
| CarbonContent Carbon Content | Carbon content from the cast/ladle analysis (mass %); unitCode P1. Replaces eusteel:mtcCarbonContent. |
| CarbonEquivalent Carbon Equivalent | Carbon equivalent value (CEV or CET), the weldability figure derived from the cast analysis (mass %); unitCode P1. Replaces eusteel:mtcCarbonEquivalent. |
| CopperContent Copper Content | Copper content from the cast analysis (mass %); unitCode P1. Replaces eusteel:mtcCopperContent. |
| Elongation | Percentage elongation after fracture (A, or Agt for reinforcing steel); unitCode P1. Replaces eusteel:mtcElongation. |
| NitrogenContent Nitrogen Content | Nitrogen content from the cast analysis (mass %); unitCode P1. Replaces eusteel:mtcNitrogenContent. |
| PhosphorusContent Phosphorus Content | Phosphorus content from the cast analysis (mass %); unitCode P1. Replaces eusteel:mtcPhosphorusContent. |
| RadiometricControl Radiometric Control | Radiometric (radioactivity) control result for the steel, in the unit the certificate states; unitCode C62. Replaces eusteel:mtcRadiometricControl. |
| RelativeRibArea Relative Rib Area | Relative rib area fR of ribbed reinforcing steel (bond performance); unitCode C62. Replaces eusteel:mtcRelativeRibArea. |
| SulfurContent Sulfur Content | Sulfur content from the cast analysis (mass %); unitCode P1. Replaces eusteel:mtcSulfurContent. |
| TensileStrength Tensile Strength | Ultimate tensile strength Rm from the tensile test; unitCode MPA. Replaces eusteel:mtcTensileStrength. |
| YieldStrength Yield Strength | Yield strength Re from the tensile test; unitCode MPA. Replaces eusteel:mtcYieldStrength. |
| YieldStrengthRatio Yield Strength Ratio | Ratio of tensile strength to yield strength Rm/Re, the k value of reinforcing steel (EN 10080; the replaced eusteel:mtcYieldStrengthRatio said Re/Rm, while the examples carried Rm/Re); unitCode C62. Replaces eusteel:mtcYieldStrengthRatio. |